https://fbcdn-sphotos-e-a.akamaihd.net/hphotos-ak-prn2/1397594_10151780075843045_672071466_o.jpg

I have attempted to cast a model using Easy Composites' Fast Cast Polyurethane Casting Resin. The cast failed as the resin did not fully cure. Half the model cured but the rest came out like thick honey, see image above. I'm not sure why this happened, but my immediate problem is, how do I clean the uncured resin goo from my mold? The mold is made of RTV silicone.

Edited 12 Years Ago by moif
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
It seems like it is a big part to cast... The reason why it cures so fast is that you probably make big batches of resin at the time...
The resin cures with a exothermal reaction, its a chemical reaction creating heat...meaning the more material you have the hotter the center of your pot will be, 
the faster the resin will cure... If you make smaller amounts at the time you should have more time, you could pour them on top of each other and they should bond 
well to each other...
Maybe warren can confirm this, because I know it works with the Fastcast PU I use, but dont know how the one from easycomposites will react

Btw great to hear you were able to clean you mould Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search