There are some tiny errors on my CFRP part and I would like to partially hide them with a final black tinted clear coat of some description with an aerosol can. I have never spray painted anything before and would like some advice of how to do it..

The CFRP part has had a final layer of clear epoxy gel coat, flattened with 120-grit wet and dry and finally 800-grit (no intermediate grit available at the moment).

Could you talk me through this? Do I use just standard plastidip black and then laquer?http://www.dipyourcar.com/forums/sho...llight-Tinting

Cheers!   
Replies
LaxFriedrichs
LaxFriedrichs
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 58, Visits: 450
Thanks CC. I wish I saw this post earlier, as I attacked it with automotive clear. There was a striking improvement, but no where near the surface quality and clarity of the resin infused laminates before I ruined them. I'll apply spin, and say it's a satin finished with a smoky coating to limit reflection.Hehe

What is so special about a booth? Limitation of humidity?
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Dust

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search