By LaxFriedrichs - 11/4/2013 2:05:27 PM

There are some tiny errors on my CFRP part and I would like to partially hide them with a final black tinted clear coat of some description with an aerosol can. I have never spray painted anything before and would like some advice of how to do it..

The CFRP part has had a final layer of clear epoxy gel coat, flattened with 120-grit wet and dry and finally 800-grit (no intermediate grit available at the moment).

Could you talk me through this? Do I use just standard plastidip black and then laquer?http://www.dipyourcar.com/forums/sho...llight-Tinting

Cheers!   
By carboncactus - 11/5/2013 6:29:47 PM

Dust