Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Black tinting CFRP
Black tinting CFRP
Post Reply
Like
3
Black tinting CFRP
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
LaxFriedrichs
LaxFriedrichs
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 58,
Visits: 450
There are some tiny errors on my CFRP part and I would like to partially hide them with a final black tinted clear coat of some description with an aerosol can. I have never spray painted anything before and would like some advice of how to do it..
The CFRP part has had a final layer of clear epoxy gel coat, flattened with 120-grit wet and dry and finally 800-grit (no intermediate grit available at the moment).
Could you talk me through this? Do I use just standard plastidip black and then laquer?
http://www.dipyourcar.com/forums/sho...llight-Tinting
Cheers!
Reply
Like
3
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
Have you got a photo of the part and said errors?
Just so you know, you wont get a good finish out of an aerosol. You might get somewhere, but will require some 1200 grit and polishing.
Plastidip is very heavy, what's you reasons for using it?
Reply
Like
3
LaxFriedrichs
LaxFriedrichs
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 58,
Visits: 450
Hi Carbon. The main errors are the impurities in a thin top coat (minuscule bubbles - why didn't I degas!) and 120-grit scratches. Unfortunately, some one borrowed my camera cable - so not photos as of yet.
I mention plastidip due to seeing people use the aerosols can to paint cars, so inferred it should be good enough quality for this application?
Actually, when I wet the surface with water it's actually not too bad. Would standard automotive lacquer fill the scratches like water does?
Edited
12 Years Ago by
LaxFriedrichs
Reply
Like
2
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
No, water hides everything. Depending on what lacqquer you use (MS, HS, UHS) you will hide different levels of scratches. If it's pretty bad, I would think about using a layer of epoxy to fill everything. Then go up the grits 120,240,400,600. Then hit it with an MS, 600grit, another layer of MS. You wont get a good finish out of an aerosol, especially clear coat. In fact, you won't even get a good finish with an HPLV if you don't have a booth. If you can manage to find a way to line a small room with polythene sheet, you can get good results.
Reply
Like
2
LaxFriedrichs
LaxFriedrichs
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 58,
Visits: 450
Thanks CC. I wish I saw this post earlier, as I attacked it with automotive clear. There was a striking improvement, but no where near the surface quality and clarity of the resin infused laminates before I ruined them. I'll apply spin, and say it's a satin finished with a smoky coating to limit reflection.
What is so special about a booth? Limitation of humidity?
Reply
Like
2
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
Dust
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search