Can I get a good surface finish without spraying gelcoat? I haven't got the funds for the spraying gun and an air compressor so that'll have to wait for now. I'm doing a small part as a first try, it's a small rectangular plate, almost a tray actually. It has a nice polished surface. I got it from IKEA for 5 quid so I won't even bother with a mold, I'll just stick it on a flat signboard, seal it so there's no undercut and just infuse it. Anyway, as I already mentioned, I was wondering whether it's possible to get a good surface finish without spraying gelcoat? Or maybe I should brush down a layer of resin, wait for it to go tacky and go on from there? Any suggestions are greatly appreciated
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
You can get a good surface without a gelcoat Wink I never use a gelcoat on the parts I make and always get good results as long as the mouldsurface is perfect and you have no leaks in the bag...

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search