	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            There is no such data on the manufacturers information we have on our roll wrapped tubes.
  To be frank, you will unlikely find that data freely available either as its a very specific application so the manufacturer is extremely unlikely to have bothered to measure those figures.
  The Tubes do use a Toray T700 fibre so you may be able to find some data out there for the raw fibre and interpolate/calculate from there.                
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |