			            officially the Epoxy tooling gel HDT is 50-60C and the putty is 70-80C.
  With smaller parts Ive got away with using it upto 90C with extensive postcuring of the mould for quite a few hours.  But it is a risk though.                
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |