By Syclone3 - 8/12/2013 4:37:55 PM
I was wondering if i could use the Epoxy Mold kit or if I had to use another special type of molding technique for resin infusion? |
By Warren (Staff) - 8/13/2013 10:40:45 AM
officially the Epoxy tooling gel HDT is 50-60C and the putty is 70-80C.
With smaller parts Ive got away with using it upto 90C with extensive postcuring of the mould for quite a few hours. But it is a risk though.
|
|