officially the Epoxy tooling gel HDT is 50-60C and the putty is 70-80C.

With smaller parts Ive got away with using it upto 90C with extensive postcuring of the mould for quite a few hours.  But it is a risk though.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Syclone3 (12/08/2013)
I was wondering if i could use the Epoxy Mold kit  or if I had to use another special type of molding technique for resin infusion?
 
Thnx, Mac


Yes. The kit is quick and easy to use. I sometimes use it for smallish parts needing a quick turn round. The only limiting factor is if you want to cure the part at high temperatures in the mould. If you are in-mould curing at ambient temperatures then no problem. I have cured at 60 (after post curing the mould first) but not sure EC would recommend that.Smile

Warren

Carbon Copies Ltd
Syclone3
Syclone3
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 3, Visits: 12
I was wondering if i could use the Epoxy Mold kit  or if I had to use another special type of molding technique for resin infusion?
 
Thnx, Mac