From my experience wet lay up will never yield perfect cosmetic parts alway hit and miss,infusion is better but not Always perfect either,regarding your laminating after because your adding resin,use 80 to 120 even if you cut into the Carbon dont worry resin is viscous enough to fill scratchs left and using these grades,and gives the surface a good bonding surface just remember to clean with acetone or sp Solent A and clean down,good luck.
|