Hi all!

I´m doing my first jobs in carbon and i´m having some problems.
When applying the first coat of resin to the mold, it won´t stick and i can´t make an even coat. When curing it starts to make voids in the middle of the mould. Probably because of the release agent. How can i fix this? I tried to make the part anyway and a got tons of holes in the surface like you can see in the photo.
http://i41.tinypic.com/14uyk9g.jpg
Any help would be appreciated.

Thank you!
Reply
wochi
wochi
Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)
Group: Forum Members
Posts: 31, Visits: 188
It´s a possibility in this last photo as i wasn´t to cautious with the cleaning. was just a test. But when i apply to the mould there is a release agent there so is it normal to do like this? If you see the carbonmods video about laminating you can see the this doesn´t happen! And if i donºt have a proper coat of resin i will have pinholes in the part!
I tried anothe coat after in this part but i overapplied resin. I could get a coat but not very eaven as there was too much resin and was dripping all over the place :S
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
wochi - 12 Years Ago
fgayford - 12 Years Ago
wochi - 12 Years Ago
wochi - 12 Years Ago
TomDesign - 12 Years Ago
wochi - 12 Years Ago
Paulh37 - 12 Years Ago
matthieutje65 - 12 Years Ago
Shaneer22 - 12 Years Ago
FLD - 12 Years Ago
wochi - 12 Years Ago
Zorongo - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search