Hi all!

I´m doing my first jobs in carbon and i´m having some problems.
When applying the first coat of resin to the mold, it won´t stick and i can´t make an even coat. When curing it starts to make voids in the middle of the mould. Probably because of the release agent. How can i fix this? I tried to make the part anyway and a got tons of holes in the surface like you can see in the photo.
http://i41.tinypic.com/14uyk9g.jpg
Any help would be appreciated.

Thank you!
Reply
wochi
wochi
Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)
Group: Forum Members
Posts: 31, Visits: 188
i tried to apply a coat on top of the part just to see the result and the same thing is happening. That´s what i get in the mould also. I can´t get an even coat of resin.

http://i42.tinypic.com/25p4j7m.jpg
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
wochi - 12 Years Ago
fgayford - 12 Years Ago
wochi - 12 Years Ago
wochi - 12 Years Ago
TomDesign - 12 Years Ago
wochi - 12 Years Ago
Paulh37 - 12 Years Ago
matthieutje65 - 12 Years Ago
Shaneer22 - 12 Years Ago
FLD - 12 Years Ago
wochi - 12 Years Ago
Zorongo - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search