Thickness- number of CF layers for motorbike fairing ?


Author
Message
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Hi,

I now have an almost mint condition MV Agusta F4 750 SR in my garage ... yeahhh ...w00t

Of course it will need a complete CF "workover" starting with all the little bits, and ending up with making a full set of CF fairings.

Now to the Q ... I'm going to build most of it using infusion, and most parts will be painted, so surface quality is not such a big concern..

How many layers of which CF fibre (I plan on at least one layer of Twaron for impact resistance on some parts) will be the best compromise between strenght and weight?

Since I'm not building this to make money, but to improve on my own bike, economy is not the biggest concern ...

I have a large stock (20 m +) of  "Satin Weave" CF 375 gsm ... So I plan to use that for most of the parts.

Any advice will be much appreciated :-)

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Replies
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi
it may be an issue with the image but the part came out quite well and the finish of the g50 was relatively flat prior to laying up the 
carbon. 

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Jess8bit
Jess8bit
Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)
Group: Forum Members
Posts: 133, Visits: 566
Bartonphoenix750 (25/07/2013)
Hi
it may be an issue with the image but the part came out quite well and the finish of the g50 was relatively flat prior to laying up the 
carbon. 
ok BigGrin
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dravis - 13 Years Ago
Warren (Staff) - 13 Years Ago
carbonfibreworks - 13 Years Ago
Dravis - 13 Years Ago
carbonfibreworks - 13 Years Ago
FLD - 13 Years Ago
baja_patient - 13 Years Ago
carbonfibreworks - 13 Years Ago
     Looks good!!
Warren (Staff) - 13 Years Ago
Jess8bit - 13 Years Ago
carbonfibreworks - 13 Years Ago
Jess8bit - 13 Years Ago
wozza - 13 Years Ago
carbonfibreworks - 13 Years Ago
Jess8bit - 13 Years Ago
morepower - 13 Years Ago
Jess8bit - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search