Hi,

I now have an almost mint condition MV Agusta F4 750 SR in my garage ... yeahhh ...w00t

Of course it will need a complete CF "workover" starting with all the little bits, and ending up with making a full set of CF fairings.

Now to the Q ... I'm going to build most of it using infusion, and most parts will be painted, so surface quality is not such a big concern..

How many layers of which CF fibre (I plan on at least one layer of Twaron for impact resistance on some parts) will be the best compromise between strenght and weight?

Since I'm not building this to make money, but to improve on my own bike, economy is not the biggest concern ...

I have a large stock (20 m +) of  "Satin Weave" CF 375 gsm ... So I plan to use that for most of the parts.

Any advice will be much appreciated :-)

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Replies
Jess8bit
Jess8bit
Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)
Group: Forum Members
Posts: 133, Visits: 566
yeah, I totally agree, and I do the same.

I was nearly sure about you using sprayed GC on this one, because I recognize slight prints through it, marking the cloth, don't know if you see what i mean. The cloth is not completely flat, due to slight spots left by the spray gun. 

This is a concern to me, as I'd like a perfect cosmetic part, and I'm looking for a solution to get rid of that. 

A solution would be to slightly sand the GC once cured, to flatten it.
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Jess8bit (25/07/2013)
yeah, I totally agree, and I do the same.

I was nearly sure about you using sprayed GC on this one, because I recognize slight prints through it, marking the cloth, don't know if you see what i mean. The cloth is not completely flat, due to slight spots left by the spray gun. 

This is a concern to me, as I'd like a perfect cosmetic part, and I'm looking for a solution to get rid of that. 

A solution would be to slightly sand the GC once cured, to flatten it.


Sounds like you are either laying down the GC50 too thick or with too much air pressure. If applied correctly you should not need to sand it before lay-up, sort of defeats the object of using it in the first place.

Carbon Copies Ltd
Edited 12 Years Ago by wozza
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dravis - 12 Years Ago
Warren (Staff) - 12 Years Ago
carbonfibreworks - 12 Years Ago
Dravis - 12 Years Ago
carbonfibreworks - 12 Years Ago
FLD - 12 Years Ago
baja_patient - 12 Years Ago
carbonfibreworks - 12 Years Ago
     Looks good!!
Warren (Staff) - 12 Years Ago
Jess8bit - 12 Years Ago
carbonfibreworks - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
Jess8bit - 12 Years Ago
morepower - 12 Years Ago
Jess8bit - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search