Group: Forum Members
Posts: 156,
Visits: 14K
|
Great work ,a lot of guys haven't a clue about composites jumping in trying run before they can walk,the basic skills and construction comes from boat building,I can not upload from this iPad would be happy to end photos through email,right now iam making air box with ram air for 03 r1 graves do a fiberglass one,but iam sure I can make my own with a better intake and more air vollum capacity,what was you total laminate thickness around mounting points, when I made mine at mounting points I had 25 layers and every 10 centimetres I tapered layers to down 25 -15 -10-5 total weight was 1046 grams a saving of over 9lkilos from the original subframe.
|