By morepower - 7/13/2013 9:38:46 AM
I have been using Advanced Composites Group's VTF261 for almost all of my Pre-preg parts surface material. I also use some material from SHD but that is for backing up the part as it is quite a bit cheaper than VTF. So after a chat with some of the guys at PRF I decided to try their PRF 464 material this week... I only got the part out of the mould last night so sorry for the poor photos but it is actually a very good product and although there is some pin holes on the surface it is more due to the breather stack we think than the material. I laid it up like I would with VTF but we think it has to have a perforated release film not the non perf I have been having the best results with VTF.
Again sorry for the poor camera phone photos I took last night. |
By 20_rc51_00 - 1/27/2014 3:32:11 AM
Thanks for the replies!
|
|