Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
graphics / logos / stickers / transfers UNDER coating epoxy
graphics / logos / stickers / transfers UNDER coating epoxy
Post Reply
Like
19
graphics / logos / stickers / transfers UNDER coating epoxy
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
benet
benet
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 59,
Visits: 373
Has anyone had any success putting graphics under epoxy.
I noticed
TomDesign had done some with AMG stickers. I tried this once with prints on clear laminate and it went so wrong i gave up. The laminate floated to the top of the coating resin becoming unstuck from the layer beneath. the print faded in colour.
TomDesign during skinning stuck his stickers directly onto rough (120?) sanded resin and then coated... does the resin seep under and hide the scrtach marks , doesnt that lead to the sticker coming unstuck and "floating" as it did with me .
Id love to put my logo under my last layer of coating resin ... any tips ?
BTW i tried rice paper ... not much joy there ... again printing and sticking issues ...
thanks
Ben
Tags
graphics
logos
skinning
stickers
transfers
Reply
Like
19
Reply
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Thank you i done lots of stickers under resin stuff.
you ask why this happened coz you use polyster resin that melt stickers and their paint with epoxy you never get things like that.
hope it help
Reply
Like
19
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
graphics / logos / stickers / transfers UNDER coating epoxy
benet
-
13 Years Ago
Thank you i done lots of stickers under resin stuff. you ask why this happened coz you use...
TomDesign
-
13 Years Ago
actuallyi was using epoxy. do you use standard clear vinyl stickers or is it a special type ? Ben
benet
-
13 Years Ago
i simply order at advertising printing company so honestly i do not know but i can ask if you need?
TomDesign
-
13 Years Ago
I have used a number of different things as logo, text or graphics under epoxy coating resin, I...
Dravis
-
13 Years Ago
thanks , i guess i'll try again.. it sounds so simple ... i think cutting away the clear...
benet
-
13 Years Ago
Post Reply
Like
19
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search