I have used a number of different things as logo, text or graphics under epoxy coating resin, I have only had very few problems ... hmmm
I used labels printed with a Brother P-touch .. I've used graphics laserprinted on to self-adhesive paper... I've used old fashion rub on "transfer letters", ordinary printed stickers ... even embroidered badges, normally used for sewing on to clothing ...
I normally cut away all the "clear" parts of stickers or "transfers" since i have seen differences in the colouring or not getting a clear, clean look of the CF under the stickers.
I coat all labels, logos or stickers with a thick coat of resin. often the parts get clear coated as well.