How would you set up vac/feed on this shape?


Author
Message
jamesw
jamesw
Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)
Group: Forum Members
Posts: 61, Visits: 558
I've come to infuse a part with a shape that's not as straightforward as the rectangular parts I've made so far - looking for suggestions on how to set up (It's pretty flat,  this is the view from top)
was thinking of feeding from the right side, and pulling vacuum from the upper 2/3's on the left... Or am I better off center feeding the resin?

http://www.talkcomposites.com/Uploads/Images/a0b1e9a9-8ca9-4d7e-8c81-a2c8.jpg
Reply
stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178

...you wrap your feed pipe in flow medium leaving a 6" overhang which you then spraytak or tape onto the existing flow medium ...


I take it you don't use a silicon connector like the one below.

Thanks
Stuart

http://www.easycomposites.co.uk/Images/products/large/Infusion-silicone-connector.jpg