I've come to infuse a part with a shape that's not as straightforward as the rectangular parts I've made so far - looking for suggestions on how to set up (It's pretty flat,  this is the view from top)
was thinking of feeding from the right side, and pulling vacuum from the upper 2/3's on the left... Or am I better off center feeding the resin?

http://www.talkcomposites.com/Uploads/Images/a0b1e9a9-8ca9-4d7e-8c81-a2c8.jpg
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
I would have the resin feed in the middle of the right hand side with the spiral running the full length and the vac outlet in the middle of the left side (so directly opposite) If you have the resin feed in the middle of the part you can get print through on the "seen side" of the part where the resin was fed in. 
Just my preferenceSmile

Carbon Copies Ltd
Edited 12 Years Ago by wozza
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search