Carbon noble bonnet (clam) with attempt at V weave


Author
Message
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
I thought Id have a go at doing a V weave with resin infusion... wasnt easy but made was pleased with the end result.

Original weighed 21kgs with lights (lights weigh 1kgs) and mine is under 8kgs so very good weight saving.

I also backed the wheel arches in kevlar as well as soric so should be resistant to start crazing.

got a coat of lacquer on the clip last night... needs flatting and a couple more coats but looks miles better already... top 2 pics are laquered, bothom ones are straight out of mould with flash lines and release agents etc.



 









and here is a pic of what I did with the car on monday Wink


Reply
WilliamsHPF
WilliamsHPF
Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)
Group: Forum Members
Posts: 26, Visits: 349
that's outstanding work!  (the 700hp)... and the carbon is nice too.

  Can't wait to see it all together and scaring old people!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
andygtt - 12 Years Ago
TomDesign - 12 Years Ago
stuart321 - 12 Years Ago
             impressive project! good job!
matthieutje65 - 12 Years Ago
Bruce - 12 Years Ago
fgayford - 12 Years Ago
alebassa - 12 Years Ago
andygtt - 12 Years Ago
WilliamsHPF - 12 Years Ago
Demlotcrew - 12 Years Ago
CarbonMike - 12 Years Ago
SebRS - 12 Years Ago
andygtt - 12 Years Ago
20_rc51_00 - 11 Years Ago
Toffee - 11 Years Ago
combustioncraig - 11 Years Ago
Toffee - 11 Years Ago
andygtt - 11 Years Ago
20_rc51_00 - 11 Years Ago
wildcard - 11 Years Ago
     Nice work!
singcomposite - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search