Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
As said if heat won't cure it, the only solution is scraping it off and re-applying fresh resin.
We always recommend that with epoxies you use the exact ratio on the bottle down to the nearest gram (or better) where possible.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|