posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Another weekend spent shaping foam and sanding body filler!! A good few coats of high build primer. A flat and polish tomorrow and should be able to take a mould from it.
Warren
Carbon
Copies Ltd
Edited
12 Years Ago by
wozza
Reply
Like
2
Reply
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
wozza (25/03/2013)
Thanks for the comments chaps. I managed to pull a GRP test piece today just to prove the mould. The duct is for a customer who wanted a specific size Intake Duct. 300mm x 220mm to take 75mm Ducting.
Looks like I will be ordering some Pre Preg don't fancy trying to infuse it.
Warren
Quality work Warren.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Intake Duct
wozza
-
12 Years Ago
Looking good! Your own variation of the NACA duct I guess.
Warren (Staff)
-
12 Years Ago
It looks good so far. That part looks like the duct used on NASCAR windows.
tauruck
-
12 Years Ago
Thanks for the comments chaps. I managed to pull a GRP test piece today just to prove the mould. The...
wozza
-
12 Years Ago
[quote][b]wozza (25/03/2013)[/b][hr]Thanks for the comments chaps. I managed to pull a GRP test...
carbonfibreworks
-
12 Years Ago
Managed to get the plug done for the top section of the Duct which will house the cone filter. The...
wozza
-
12 Years Ago
Managed to get the prototype duct finished.
wozza
-
12 Years Ago
That looks excellent , did you use infusion Warren ? Chris
carbonfibreworks
-
12 Years Ago
Hi Wozza Looks nice. How did you do the graphics exactly? Thanks Fred
fgayford
-
12 Years Ago
Hi Chris, this one was wet laid but future ones will be done by Infusion. I don't do much wet lay...
wozza
-
12 Years Ago
Hi Fred, I have a basic cheap Chinese Vinyl Cutter/Plotter which I use to cut out the text....
wozza
-
12 Years Ago
Thanks Warren Graphics well done, add so much to the look of a piece. Fred
fgayford
-
12 Years Ago
Opinions please! I wasn't happy with the "edge" on the front of the Intake so I decided to make up...
wozza
-
12 Years Ago
[quote][b]wozza (10/04/2013)[/b][hr]Opinions please! I wasn't happy with the "edge" on the front of...
carbonfibreworks
-
12 Years Ago
Hi Chris how did your day spannering go ? The simulation shows a slight increase in air flow with...
wozza
-
12 Years Ago
We had a great day at Mallory, the two bikes had minor problems but we managed to take care of them...
carbonfibreworks
-
12 Years Ago
Looks good! I did notice however, the course surface on the inside where the air will be flowing. I...
baja_patient
-
12 Years Ago
Thanks for the feedback. I think it may be the picture quality. :) The inside has had a coat of...
wozza
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search