Hi,

I am a new member here so I hope no one has asked this before.

Working within a hospital we use Pre-Preg for all of our Carbon Fiber uses.

The main reason for this is the quality of the end product and even thickness of resin.

 

I was looking at making a mold but the mold needs to be heat resistant. Had a hunt around on the net and found this stuff “Mold Max 60” – High Heat Resistant Silicone Rubber Mold system.

 

Has anyone tried this stuff before?

Cheers.
Reply
Brad 612
Brad 612
Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)
Group: Forum Members
Posts: 2, Visits: 14
Hi I am looking for info on methods to make carbon fibre moulds to be used in the plastic rotational moulding process,we have fibre glass mouldings 
With flanges that would directly make the finished moulds in cf,the questions are what would be the best resin to use at high  temperature  and what would be a good finished mould thickness to allow for long life and fast heating in the process oven, any advice will be appreciated brad
Edited 12 Years Ago by Brad 612
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search