By calgone - 2/11/2013 4:06:34 PM
Hi,
I am a new member here so I hope no one has asked this before.
Working within a hospital we use Pre-Preg for all of our Carbon Fiber uses.
The main reason for this is the quality of the end product and even thickness of resin.
I was looking at making a mold but the mold needs to be heat resistant. Had a hunt around on the net and found this stuff “Mold Max 60” – High Heat Resistant Silicone Rubber Mold system.
Has anyone tried this stuff before?
Cheers.
|
By pk_090 - 3/7/2013 1:13:25 PM
Geesh sounds like the hospital is well kitted out then! i wish i had those kind of facilities!
|
|