Infusion resin calculation chart


Author
Message
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Hey Paul, 

On your instructional thread theres a chart calculating resin needed for a certain size part. Am I missing something because on the infusion starter kit instructions there is a similar chart but with much smaller amounts. 

I have a first test going at the moment, part is about 34x24cm 2 layers 200gm carbon and 2 layers 160g (i think it is) E-glass. 

I was thinking like 250g resin or will I need more?

cheers,

Regards,

Fabian 
Reply
Paul (Staff)
Paul (Staff)
Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Fabian,

Trust the chart on here, the Infusion PDF guide requires an update, as long as you are watching the infusion even is you mix too little resin you can effectivly 'pause' the infusion by clamping both feed and vacuum lines while you mix a bit more resin.  But you are about spot-on with 250g so that's where I would start.

Paul Statham
Easy Composites / Carbon Mods - Technical
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search