Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Number of layers?
Number of layers?
Post Reply
Like
3
Number of layers?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
pedcrist
pedcrist
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 42,
Visits: 350
Hi,
I have a project to do, wich is a full front of a Honda Civic(Hood, bumper and fenders), in one piece, with CF.
What is your opinion about the the number of layers and type of CF to use?
Pedro
Edited
12 Years Ago by
pedcrist
Reply
Like
3
Reply
pedcrist
pedcrist
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 42,
Visits: 350
Thanks, Warren.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Number of layers?
pedcrist
-
12 Years Ago
Does someone give a help?
pedcrist
-
12 Years Ago
It is difficult to say without knowing how curved the panels are. On some highly curved panels, a...
Warren (Staff)
-
12 Years Ago
Thanks, Warren.
pedcrist
-
12 Years Ago
Warren-- do you know of any charts we can all use for us to memorize for thickness per layer of a...
brasco
-
12 Years Ago
i thought this may help you work out how to make your molds. i dont have much to add for sorting...
brasco
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search