A customer has asked me to look into making some fenders (mudguards) for a Trials bike and I was thinking of giving your flexible resin a try.
Couple of questions though?

1- Can the Resin be used for Infusion.
2- Is your GC50 compatible with the resin and will it still allow the part to flex without cracking/de-laminating.

Thanks in advance Warren

Carbon Copies Ltd
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
If you're anywhere near macclesfield I have a dribble left over you can have if you want to make a sample to see what its like.