Hi Warren,
I agree with FLD; I think it would be too thick to infuse (although it may be possible, through a very easy flowing laminate) but I would certainly not recommend teaming it up with the GC50. Although they may bond, you would would be throwing away the flexibility of the EF80 and ending up with a laminate that would bend (from the EF80) when the GC50 gelcoat, although very resilient in normal use, would certainly crack away given enough punishment.
A lot of people have found that the EF80 wets out fibre so well that you can get great looking results just by wet-lay laminating it so you won't need to infuse and the surface finish is good enough to not need a gel. I too think that on its own, with the right choice of reinforcement, it might be a good system for some really durable parts.
All the best, Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|