I thinking in how can do a split mould on to these motorcycle saddlebag, where I split... any help I will appreciate

Greetings from Chile
torsten Ker
t
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 59, Visits: 278
I guess the bag hat to be rigid and think you will have no other choice to make 5 part mould, each side and bottom or it will be a challenge to get the saddlebag out

The problem is the straight sided and the overlap on the bottom to one side

J. P.
J. P.
Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)
Group: Forum Members
Posts: 11, Visits: 55
torsten Ker - 11/5/2020 10:10:47 PM
I guess the bag hat to be rigid and think you will have no other choice to make 5 part mould, each side and bottom or it will be a challenge to get the saddlebag out

The problem is the straight sided and the overlap on the bottom to one side

I was thinking in 3, the side and front, the rear and the back, and bottom... but i'm not sure if can take out

torsten Ker
t
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 59, Visits: 278
yes, you are right, that may work but I think not to make the mould to stiff and be carefull not to crack the gelcoat on demoulding

J. P.
J. P.
Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)
Group: Forum Members
Posts: 11, Visits: 55
torsten Ker - 11/5/2020 10:26:21 PM
yes, you are right, that may work but I think not to make the mould to stiff and be carefull not to crack the gelcoat on demoulding

I would do in fiberglass, I check your video, but I don't if I must to do with the mould open and leave a dry fiberglass for close and seal from inside?

Thanks for your advice

torsten Ker
t
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 59, Visits: 278
I have 3 and 4 part moulds, created flanges which have a 2cm polished flat (like a U Channel profile) on the edges outside and I seal them with gum tape  only having to put a bag into the indise as usual
Other people bag a mould like this as a mould which is definetly easier but time consuming with more bagging required

Edited 6 Years Ago by torsten Ker
J. P.
J. P.
Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)
Group: Forum Members
Posts: 11, Visits: 55
torsten Ker - 11/5/2020 10:46:52 PM
I have 3 and 4 part moulds, created flanges which have a 2cm polished flat (like a U Channel profile) on the edges outside and I seal them with gum tape  only having to put a bag into the indise as usual
Other people bag a mould like this as a whole mould which is definetly easier but time consuming with more bagging required

but this is without bag, is fiberglass no carbon fiber... 

torsten Ker
t
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 59, Visits: 278
have you thought about doing 2 parts , angeling the sides/rounding and glueing them together with glassfibre tape
One mould for the back and one for the font
A single multipart usuable mould will be a lot of work

You could then sand off the seam edges, fill them abit and spray the lot
much easier that way

I did that on 1989 for bike saddle bags with polyester and hand layup :-)

Edited 6 Years Ago by torsten Ker
J. P.
J. P.
Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)Supreme Being (144 reputation)
Group: Forum Members
Posts: 11, Visits: 55
torsten Ker - 11/5/2020 11:15:31 PM
have you thought about doing 2 parts , angeling the sides/rounding and glueing them together with glassfibre tape
One mould for the back and one for the font
A single multipart usuable mould will be a lot of work

You could then sand off the seam edges, fill them abit and spray the lot
much easier that way

I did that on 1989 for bike saddle bags with polyester and hand layup :-)

I will try, do you have pics about it?

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
3 part mould, no problem.