Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pre-Pregs
»
Removing backer film
Removing backer film
Post Reply
Like
6
Removing backer film
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
nc42
nc42
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 23,
Visits: 365
I'm making a large number of small prepreg parts. I'm wondering if anyone has suggestions to facilitate the removal of the backing film from prepregs and glue films (I'm using XC110). I've been using freeze spray which works well but isnt particularly sustainable. I've also tried nicking an edge which works buy is quite slow. Any secret tips out there to quickly/easily remove backer film?
Reply
Like
6
Reply
Chris Rogers
C
Chris Rogers
posted 6 Years Ago
ANSWER
HOT
Post Details
C
Group: Forum Members
Posts: 120,
Visits: 933
Instead of freeze spray you could use an aluminum block that you keep in the freezer and take out to use. It's not ideal because of the condensation but can be helpful if freeze spray isn't an option. I had one about the size of a soda can covered in adhesive teflon but a zip-lock bag would do too. That and a small Exacto-knife works pretty well.
Never tried it but could a cold-block and (clean) compressed air from a small blow-gun work?
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Removing backer film
nc42
-
6 Years Ago
Instead of freeze spray you could use an aluminum block that you keep in the freezer and take out to use. It's not ideal because of the condensation but can be helpful if freeze spray isn't an option...
explorecomposites
-
6 Years Ago
always been using a scalpel blade for me, or a bit of freeze spray on the sticky tooling preg.
scottracing
-
6 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search