Successfuly made some pre preg. Wanting to clear coat. Untill I get set up I'm using rattle can acrylic.

I key in with 800 grit but it drys showing all the 800 scratches .

Would this still happen with proper mixed 2k clear coat?

Thanks
Replies
LibertyMKiii
L
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 19, Visits: 110
This one was wet sanded with 600 grit then 2k clear was applied.


carbon man
carbon man
Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
LibertyMKiii - 7/17/2020 5:22:54 PM
This one was wet sanded with 600 grit then 2k clear was applied.


Nice! I take that's dried and polished. Air a standard face ok to use. Or do you use air feed? 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carbon man - 5 Years Ago
Hanaldo - 5 Years Ago
carbon man - 5 Years Ago
beliblisk - 5 Years Ago
carbon man - 5 Years Ago
beliblisk - 5 Years Ago
Hanaldo - 5 Years Ago
LibertyMKiii - 5 Years Ago
carbon man - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search