Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
XCR, being a resin, is a much thicker layer. Properly sanded smooth XCR with a high quality polish will look very good but generally does not look as "wet" as a clear coat lacquer.
Also Modern automotive lacquers will generally offer much better UV protection as most are 100% UV stable. Depending on your climate, this may or may not be a consideration.