Group: Forum Members
Posts: 4,
Visits: 5
|
Hi,
I am making a resin river table where the river will be approximately 50mm deep.
I see your glasscast 50 resin is for 25mm deep as a maximum and wondered whether you can pour additional 25mm on the first 25mm pour when it reaches the B cure stage or whether this would be too much resin curing at the same time.
Is it best to pour a second 25mm pour on top of the first 25mm pour at the B cure stage, or is it best to sand the surface to key it and then pour the second 25mm pour?
Many thanks
|