There is a youtube video of a guy who shows you how to make your own prepreg, he claims it is better than store bought.
Check "How to make your own prepreg" David Algie is his name. He was chief fabricator for a formula racing team. He is also making an all carbon fiber airplane. Its worth looking into, I have learned a lot from him.
I made an autoclave for $600.00 out of an old industrial sized paint pressure pot. It is 60 gallons large. Good for 110psi