When doing a complex part that would need prepreg or profinish, what about wetting one layer of cf, leaving it down until just tacky, applying it in the mould with cuts and so on like with prepreg and then going on like for standard infusion with the other dry layers, bagging and infusing?? Anybody tried this?
Alessandro
|