By Leon - 11/14/2012 8:45:53 AM
Hi guys,
This is good video that cover the entire steps of pre-preg may can help you
http://www.youtube.com/watch?v=J9tF7TeAYwM&feature=relmfu
Regads
Leon
|
By fgayford - 3/23/2013 5:55:02 PM
I would guess your going to have a fail. Once gelled its gelled. I think you could get away with brushing a layer of resin in the mould and apply dry fabric when it has gelled.