Warren (Staff) - 9/4/2019 8:38:49 AM
Although in theory it will work as a filler, the results will not give you a hidden unseen repair.  The best way to repair damaged gelcoat is with fresh gelcoat. That way once blended in and polished, you should have a seamless repair that matches the original. 

So just use gelcoat with hardner?

Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Although in theory it will work as a filler, the results will not give you a hidden unseen repair.  The best way to repair damaged gelcoat is with fresh gelcoat. That way once blended in and polished, you should have a seamless repair that matches the original. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
Can use  this filler to repair gelcoat on uni mould system?