By Classicarbon - 9/4/2019 6:46:20 AM

Can use  this filler to repair gelcoat on uni mould system?
By Classicarbon - 9/4/2019 8:40:59 AM

Warren (Staff) - 9/4/2019 8:38:49 AM
Although in theory it will work as a filler, the results will not give you a hidden unseen repair.  The best way to repair damaged gelcoat is with fresh gelcoat. That way once blended in and polished, you should have a seamless repair that matches the original. 

So just use gelcoat with hardner?