Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Although in theory it will work as a filler, the results will not give you a hidden unseen repair. The best way to repair damaged gelcoat is with fresh gelcoat. That way once blended in and polished, you should have a seamless repair that matches the original.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|