Will the gauge on catch can will be enough to check drop test on infiusion ?or I need other gauge on the pump?

I plan to get starter kit for infiusion and catch can got the gauge.
Thanks
Reply
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Yes, the gauge on the catch pot is okay to use and observe when drop-testing. It's not uncommon to see a bit of vaccum loss on the catch pot over a period of time, though, so pull full vacuum on it just before testing your bag

 