Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Pressure drop test on infiusion
Pressure drop test on infiusion
Post Reply
Like
3
Pressure drop test on infiusion
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Classicarbon
C
Classicarbon
posted 6 Years Ago
ANSWER
HOT
Topic Details
C
Group: Forum Members
Posts: 86,
Visits: 639
Will the gauge on catch can will be enough to check drop test on infiusion ?or I need other gauge on the pump?
I plan to get starter kit for infiusion and catch can got the gauge.
Thanks
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Pressure drop test on infiusion
Classicarbon
-
6 Years Ago
Yes, the gauge on the catch pot is okay to use and observe when drop-testing. It's not uncommon to see a bit of vaccum loss on the catch pot over a period of time, though, so pull full vacuum on it.....
MarkMK
-
6 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search