8/9/2019 9:29:50 AM
Will the gauge on catch can will be enough to check drop test on infiusion ?or I need other gauge on the pump?
I plan to get starter kit for infiusion and catch can got the gauge.
Thanks
By MarkMK
-
8/10/2019 2:02:24 PM
Yes, the gauge on the catch pot is okay to use and observe when drop-testing. It's not uncommon to see a bit of vaccum loss on the catch pot over a period of time, though, so pull full vacuum on it just before testing your bag