Zero Leak Vacuum Infusion


Author
Message
leeks
l
Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)
Group: Forum Members
Posts: 7, Visits: 3.7K
Hi All,

I've been infusing for a few years now and recently I've purchased a Greisinger GDH absolute gauge. My question is, when everyone says they get a perfect leak proof bag - is it really? Is there an acceptable tolerance for a leak to still be considered perfect?

Obviously the volume/size of the part being infused is relevant so after multiple tests envelope bagging a 1m2 glass mould with about 1mm thick laminate + flow media. I've had leaks ranging from 1mbar/hour to 10mbar/hour.

I've been under the impression that a perfect seal means it should keep the same vacuum for days on end. Is this asking too much?

The parts I'm infusing are cosmetic carbon so avoiding any pin holes or bubbles is the goal.

Thank you.

Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Good post Chris, lots of good info. All though for the record, I do this for a living and I ALWAYS clamp the vac pump and shut it off after the infusion has completed 🤠
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
leeks - 6 Years Ago
oekmont - 6 Years Ago
Hanaldo - 6 Years Ago
oekmont - 6 Years Ago
Hanaldo - 6 Years Ago
oekmont - 6 Years Ago
leeks - 6 Years Ago
8900120dd - 6 Years Ago
oekmont - 6 Years Ago
8900120dd - 6 Years Ago
leeks - 6 Years Ago
Designbikes - 6 Years Ago
explorecomposites - 6 Years Ago
Designbikes - 6 Years Ago
Warren (Staff) - 6 Years Ago
Hanaldo - 6 Years Ago