Hello

I am thinking of making a fiber glass-broody composite with 50 grams fiber glass surface tissue ...and I want to make the composite so thin .about .0.5 mm and use the minimum amount of resin. The question here.. still i need to use mesh or the resin can flow in this surface tissue alone. Thanks
Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
No, without flow media this will not work. Finer cloth usually has lower resin flow propertys than thicker cloth.
The pump will work just fine. If your setup is airtight it doesn't matter how big your pump is. Look that you don't trap too much air when sealing the bag, so the pump doesn't take too long pulling the bag down initially.