Hi all

Am making a router table and used Glascast 30 to get a smooth level finish. Most of the table is ok but part has gone a bit orange peely. But also, I thought I had enough to cover the table but I am approx 1mm short on depth in parts. So I need to top up.
Am I best to key sandpaper the layer I have put down to provide a key, or am I ok to pour more Glasscast 3 on top as is?

Many thanks.

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
IPA wipes or acetone should be fine on fully cured resin. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search