			            Hi all
  Am making a router table and used Glascast 30 to get a smooth level finish. Most of the table is ok but part has gone a bit orange peely. But also, I thought I had enough to cover the table but I am approx 1mm short on depth in parts. So I need to top up. Am I best to key sandpaper the layer I have put down to provide a key, or am I ok to pour more Glasscast 3 on top as is?