By Jemm0 - 6/24/2019 7:40:49 PM
Hi all
Am making a router table and used Glascast 30 to get a smooth level finish. Most of the table is ok but part has gone a bit orange peely. But also, I thought I had enough to cover the table but I am approx 1mm short on depth in parts. So I need to top up. Am I best to key sandpaper the layer I have put down to provide a key, or am I ok to pour more Glasscast 3 on top as is?
Many thanks.
|
By Warren (Staff) - 6/26/2019 11:10:01 AM
IPA wipes or acetone should be fine on fully cured resin.
|
|