I had these parts made for a project I am working on and the manufacturer claims they are 'autoclave dry carbon', which should mean pre-preg, but to my untrained eye it looks like regular vacuum bagged wet infusion. There are tiny bubbles along the edges and the outer clear resin layer seems thicker than what I would expect a pre-preg.

Are there any carbon experts out there that can help me identify what process they used to make these parts?

       
Replies
Charles Woo
Charles Woo
Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)
Group: Forum Members
Posts: 5, Visits: 20
Thanks for your help guys. I really appreciate it.
Learned a lot. I didn’t know that prepreg could be so resin rich.
JasonFL
JasonFL
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 51, Visits: 707
Look up debulking during an autoclave layup. Slowly removes excess resin and air over time to ensure the plys stay uniform and the desired resin to weight ratio is hit.

Jason
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Charles Woo - 6 Years Ago
oekmont - 6 Years Ago
Charles Woo - 6 Years Ago
oekmont - 6 Years Ago
Charles Woo - 6 Years Ago
oekmont - 6 Years Ago
Charles Woo - 6 Years Ago
JasonFL - 6 Years Ago
Charles Woo - 6 Years Ago
JasonFL - 6 Years Ago
Jason B - 5 Years Ago
Hanaldo - 5 Years Ago
Jason B - 5 Years Ago
MarkMK - 5 Years Ago
Hanaldo - 5 Years Ago
matthieutje65 - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search