Group: Forum Members
Posts: 51,
Visits: 707
|
Agreed with Oek. You’d see the flow media marks on the back if it was resin infusion.
You can see the release film marks on the back surface from traditional bagging with breather cloth. Looks like a very resin rich prepreg layup that either bridged on the fine edges and/or had resin pooling in the corners.
Jason
|